Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 798 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 5.50 - 38.0 MPa
798 - 5510 psi
Average value: 20.6 MPa Grade Count:8
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Flexural Yield Strength 5.50 MPa

@Strain 0.200 %
798 psi

@Strain 0.200 %
ASTM D790
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Flexural Yield Strength 5.50 MPa

@Strain 0.200 %
798 psi

@Strain 0.200 %
ASTM D790
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
Flexural Yield Strength 5.50 MPa

@Strain 0.200 %
798 psi

@Strain 0.200 %
ASTM D790
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
Flexural Yield Strength 5.50 MPa

@Strain 0.200 %
798 psi

@Strain 0.200 %
ASTM D790
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..