Mechanical Properties Metric English Comments
Flexural Yield Strength 53.4 MPa
7750 psi
ASTM D790
IRPC Polimaxx Polene 1111NX TA4 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% TALCUM REINFORCEDAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES