Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 53.4 MPa | 7750 psi | ASTM D790 |
IRPC Polimaxx Polene 1111NX TA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% TALCUM REINFORCEDAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |