Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 53.0 MPa @Thickness 6.40 mm |
7680 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Flexural Yield Strength | 53.0 MPa @Thickness 6.40 mm |
7680 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |