Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 53.0 MPa | 7690 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 53.0 MPa | 7690 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XTWE265 ASA (Asia Pacific) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware. |
|||
Flexural Yield Strength | 53.0 MPa | 7690 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 53.0 - 168 MPa @Temperature -40.0 - 80.0 °C |
7690 - 24400 psi @Temperature -40.0 - 176 °F |
Average value: 114 MPa Grade Count:1 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Flexural Yield Strength | 53.0 MPa | 7690 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Flexural Yield Strength | 53.0 MPa | 7690 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Flexural Yield Strength | 53.0 MPa | 7690 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Flexural Yield Strength | 53.0 MPa @Thickness 6.40 mm |
7680 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Flexural Yield Strength | 53.0 MPa @Thickness 6.40 mm |
7680 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |