Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 74.6 MPa | 10800 psi | ASTM D790 |
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Flexural Yield Strength | 74.6 MPa | 10800 psi | ASTM D790 |
RedEye On Demand VeroWhite PolyJet Resin White for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Flexural Yield Strength | 74.6 MPa | 10800 psi | 15 mm/min; ASTM D790 |
LG Chemical MI-730 MIPS |