Polymer Property : Flexural Yield Strength = 10800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 74.5 MPa
10800 psi
ASTM D790
Ravago Manufacturing Americas Hylac® HF143 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Yield Strength 74.6 MPa
10800 psi
ASTM D790
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping
Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero..
Flexural Yield Strength 74.6 MPa
10800 psi
ASTM D790
RedEye On Demand VeroWhite PolyJet Resin White for Rapid Prototyping
Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero..
Flexural Yield Strength 74.5 MPa

@Thickness 3.20 mm
10800 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 74.5 MPa

@Thickness 3.20 mm
10800 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 74.5 MPa
10800 psi
ASTM-D790
Ineos ABS Lustran® 451 ABS, Injection Molding Grade
Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss.
Flexural Yield Strength 74.6 MPa
10800 psi
15 mm/min; ASTM D790
LG Chemical MI-730 MIPS
Flexural Yield Strength 74.5 MPa

@Thickness 3.20 mm
10800 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
Flexural Yield Strength 74.5 MPa

@Thickness 3.20 mm
10800 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 74.5 MPa
10800 psi
ASTM D790
GRECO ISOPAK 547HF ABS Resin
High Flow GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Flexural Yield Strength 74.5 MPa
10800 psi
5% strain; ASTM D790
Metton LMR M1539 Liquid Molding Resin
Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can ..
Flexural Yield Strength 74.5 MPa
10800 psi
5% strain; ASTM D790
Metton LMR M2100VO Liquid Molding Resin
Metton LMR is a tough and durable engineering plastic material used to produce large or thick molded parts for many diversified applications. The Metton LMR reaction injection molding process can ..
Flexural Yield Strength 74.5 MPa

@Thickness 3.20 mm
10800 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical XR407E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by..
Flexural Yield Strength 74.5 MPa
10800 psi
ASTM D790
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass
Information provided by Star Plastics, Inc.
Flexural Yield Strength 74.5 MPa
10800 psi
ASTM D790
Techmer ES Luriblend® POM CO E TL20
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance and CopolymerProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Yield Strength 74.5 MPa
10800 psi
ASTM D790
PlastxWorld CEVIAN® S3100 PC/ABS alloy
Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Yield Strength 74.5 - 220 MPa
10800 - 31900 psi
Average value: 151 MPa Grade Count:46
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled