Mechanical Properties Metric English Comments
Flexural Yield Strength 353 MPa
51200 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UX06003 PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UX06003 is a compound based on Polyphalamide resin containing Carbon Fiber. Added features include Electrically Conductive, Mold Release, Heat Stabilized.