Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 45.0 - 350 MPa @Temperature 120 - 275 °C |
6530 - 50800 psi @Temperature 248 - 527 °F |
Average value: 151 MPa Grade Count:11 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |