Mechanical Properties Metric English Comments
Flexural Yield Strength 349 MPa
50600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber.