Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 349 MPa | 50600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber. |