Polymer Property : Flexural Yield Strength = 5.45 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 5.45 - 607 MPa
790 - 88000 psi
Average value: 114 MPa Grade Count:182
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..