Mechanical Properties Metric English Comments
Flexural Yield Strength 326 MPa
47300 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10
LNP THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.