Polymer Property : Flexural Yield Strength = 41000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 160 - 283 MPa
23200 - 41000 psi
Average value: 235 MPa Grade Count:11
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Flexural Yield Strength 234 - 283 MPa
34000 - 41000 psi
Average value: 256 MPa Grade Count:6
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Flexural Yield Strength 103 - 283 MPa
15000 - 41000 psi
Average value: 135 MPa Grade Count:8
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Flexural Yield Strength 90.0 - 283 MPa
13100 - 41000 psi
Average value: 190 MPa Grade Count:133
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..