Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 45.0 - 380 MPa | 6530 - 55100 psi | Average value: 285 MPa Grade Count:18 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Flexural Yield Strength | 89.0 - 380 MPa @Temperature -40.0 - 121 °C |
12900 - 55100 psi @Temperature -40.0 - 250 °F |
Average value: 186 MPa Grade Count:9 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |