Polymer Property : Flexural Yield Strength = 38.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 38.2 MPa

@Thickness 6.40 mm
5550 psi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL GP1000FC Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Flexural Yield Strength 38.2 MPa

@Thickness 6.40 mm
5550 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL HI5205R PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Flexural Yield Strength 38.2 MPa
5550 psi
ASTM D790
IRPC Polimaxx Polene 2511PCX TA6 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES
Flexural Yield Strength 38.2 MPa
5550 psi
ASTM D790
IRPC Polimaxx Polene 2564PCX TA6 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTH CONTAIN UV STABILIZER AND LONG TERM HEAT AGING ADDITIVESAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ..
Flexural Yield Strength 38.2 MPa

@Thickness 6.40 mm
5550 psi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL GP3156F Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided ..
Flexural Yield Strength 38.2 MPa
5550 psi
ASTM D790
IRPC Polimaxx Polene 2563PCX TA6 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTH, CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES