IRPC Polimaxx Polene 2564PCX TA6 Polypropylene Compound

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 2564PCX TA6 Polypropylene Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTH CONTAIN UV STABILIZER AND LONG TERM HEAT AGING ADDITIVESAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Yield Strength 38.2 MPa
5550 psi
ASTM D790
Flexural Modulus 3.40 GPa
493 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Temperature 23.0 °C
0.918 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648
Users viewing this material also viewed the following: