Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 25.0 - 25.0 MPa @Temperature 90.0 - 90.0 °C |
3630 - 3630 psi @Temperature 194 - 194 °F |
Average value: 25.0 MPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |