Polymer Property : Flexural Yield Strength = 3630 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 25.0 MPa

@Temperature 90.0 °C
3630 psi

@Temperature 194 °F
ISO 178, ASTM D790
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
Flexural Yield Strength 25.0 - 25.0 MPa

@Temperature 90.0 - 90.0 °C
3630 - 3630 psi

@Temperature 194 - 194 °F
Average value: 25.0 MPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Flexural Yield Strength 25.0 - 28.0 MPa
3630 - 4060 psi
Average value: 26.8 MPa Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Flexural Yield Strength 25.0 - 207 MPa

@Temperature -40.0 - 120 °C
3630 - 30000 psi

@Temperature -40.0 - 248 °F
Average value: 84.2 MPa Grade Count:6
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Flexural Yield Strength 25.0 MPa
3630 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C
LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers.
Flexural Yield Strength 25.0 - 360 MPa
3630 - 52200 psi
Average value: 94.7 MPa Grade Count:85
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..