Mechanical Properties Metric English Comments
Flexural Yield Strength 237 MPa
34400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS
LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr..
Flexural Yield Strength 237 MPa
34400 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66
LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Flexural Yield Strength 237 MPa
34400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.