Mechanical Properties Metric English Comments
Flexural Yield Strength 53.1 - 339 MPa
7700 - 49200 psi
Average value: 208 MPa Grade Count:25
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..