Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 0.0750 - 3.17 MPa | 10.9 - 460 psi | Average value: 0.641 MPa Grade Count:63 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |