Polymer Property : Flexural Yield Strength = 10.9 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 0.0750 - 3.17 MPa
10.9 - 460 psi
Average value: 0.641 MPa Grade Count:63
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..