Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 199.7 MPa | 28960 psi | ASTM D790 |
Plenco 51130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform.. |