Flexural Yield Strength 198 MPa
28700 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific)
LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.This data was suppli..