Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 130 - 265 MPa | 18900 - 38400 psi | Average value: 182 MPa Grade Count:42 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Flexural Yield Strength | 49.987 - 265 MPa @Temperature -40.0 - 121 °C |
7250.0 - 38400 psi @Temperature -40.0 - 250 °F |
Average value: 147 MPa Grade Count:5 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |