Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 15.0 - 15.0 MPa @Temperature 90.0 - 90.0 °C |
2180 - 2180 psi @Temperature 194 - 194 °F |
Average value: 15.0 MPa Grade Count:1 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |