Mechanical Properties Metric English Comments
Flexural Yield Strength 1400 MPa
203000 psi
Hexcel® HexPly® EH04 Epoxy Resin System, IM4 Fiber
IM4 120 24" EH04 31%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel
Flexural Yield Strength 1400 MPa
203000 psi
EN2562
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm
Fiber mass: 150 g/m2Information provided by HexCel