Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 45.0 - 172 MPa | 6530 - 25000 psi | Average value: 75.2 MPa Grade Count:34 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Flexural Yield Strength | 48.0 - 172 MPa | 6960 - 24900 psi | Average value: 76.4 MPa Grade Count:15 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |