Mechanical Properties Metric English Comments
Flexural Yield Strength 139 MPa
20200 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
Flexural Yield Strength 139 MPa
20200 psi
ASTM D790
Techmer ES HiFill® PSU GF10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Yield Strength 139 MPa
20200 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS
Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 139 MPa
20200 psi
Phenolic 27%, Graphite fabric 73%
Phenolic - "91LD". Graphite fabric - "WCB"