Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 60.0 - 121 MPa | 8700 - 17600 psi | Average value: 80.4 MPa Grade Count:20 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |