Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 65.0 MPa | 9430 psi | ASTM D882 |
DuPont™ Dartek® F-101 Nylon 6,6 Forming Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A cast nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylen diamine. It contains all the excellent properties .. |
|||
Film Tensile Strength at Break, TD | 65.0 MPa | 9430 psi | ISO 1184 |
SIDPEC EGYPTENE® HD 5301 FB HDPE Film Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi.. |