Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 43.9 MPa | 6370 psi | |
Dow AFFINITY™ FM 1570 Polyolefin Plastomer AFFINITY® FM 1570 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide film products with excellent sealability and high hot tack strength, outstanding blown film optics, and .. |