Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 13.0 - 40.0 MPa | 1890 - 5800 psi | Average value: 24.4 MPa Grade Count:138 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Film Tensile Strength at Break, TD | 33.1 - 40.0 MPa | 4800 - 5800 psi | |
3M 6145 Kraft Light Duty Reinforced Water Activated Tape 3M™ Light Duty Reinforced Water Activated Tape 6145 is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and a high tack water-activated .. |