Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 51.7 MPa | 7500 psi | |
Dow Elite® 5400 Linear Low Density Polyethylene 5400 enhanced polyethylene resin is a copolymer produced via INSITE technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and optical prop.. |