Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 4.60 MPa
667 psi
ASTM D5035
3M GM110 Gripping Material
3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM 110 consists of a high-friction surface with a nylon knit backing that provides stretch..