Polymer Property : Film Tensile Strength at Break, TD = 28.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 28.8 MPa
4180 psi
ASTM D882
ExxonMobil LL 1002.32 Cast Film Resin  (discontinued **)
LL 1002.32 is a butene LLDPE resin designed for the cast film process. Films made from LL 1002.32 have very good tensile and toughness properties.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 28.8 MPa
4180 psi
ASTM D882
LyondellBasell Plexar® PX3236 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a..