Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 18.9 MPa | 2740 psi | ASTM D882 |
LyondellBasell Ultrathene® UE637000 Ethylene Vinyl Acetate Copolymer, Film Extrusion Grade ULTRATHENE UE637000 is an EVA copolymer with good toughness, flexibility and clarity. Applications include laminating and heavy duty films as well as injection and blow molding. UE637000 contains no.. |