Film Tensile Strength at Break, TD 170 MPa
24700 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 36MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film acrylic coated on one side, one side PVdC. Provides outstanding performances on all packaging machines.Availability: Africa ..
Film Tensile Strength at Break, TD 170 MPa
24700 psi
7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method
ExxonMobil Oppalyte™ 50MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & ..