Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 22.7 MPa | 3290 psi | ASTM D882 |
Chevron Phillips MarFlex® 9608 HDPE Coating Blend Resin Resin Type: Coating Blend ResinCharacteristics: Low Gel Levels, Improves MVTR, Reduces COF, Excellent Draw Properties, Excellent Processability, Improves Scuff Resistance, Improves Stiffness Propert.. |
|||
Film Tensile Strength at Break, TD | 22.7 - 27.4 MPa | 3290 - 3970 psi | |
3M 6145 White Light Duty Reinforced Water Activated Tape 3M™ Light Duty Reinforced Water Activated Tape 6145 is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and a high tack water-activated .. |