Polymer Property : Film Tensile Strength at Break, TD = 20.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 20.8 MPa
3010 psi
ASTM D882
ExxonMobil LD 313.NF Blown Film Resin
LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr..