Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 128 MPa | 18600 psi | ASTM D882 |
Solvay Specialty Polymers Ajediumâ„¢ Films -- Polyetherimide Polyether Imide (PEI) Films of polyetherimide (PEI) are amorphous and suitable for high temperature applications. They have an excellent combination of thermal, mechanical and electrical properties, along with very low f.. |