Polymer Property : Film Tensile Strength at Break, TD = 12100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 83.4 MPa
12100 psi
ASTM D882
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK)
AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc..
Film Tensile Strength at Break, TD >= 83.3 MPa
>= 12100 psi
300 N/10mm
Dr. D. Mueller Flexiso® DMD FI 14010 00360 Polyester Electrical Insulation
Structure: Flexiso® DMD, FI 14010 00360 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with ..