Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 75.8 MPa | 11000 psi | ASTM D882 |
Honeywell Stretch-Vac® 2000 Heat-Stabilized Blown Film
(discontinued **) Description: Stretch-Vac® 2000 is a pink tinted, high elongation, heat-stabilized blown film produced from modified polyamide resin. It is available in widths up to 80 inches as layflat tubing and.. |
|||
Film Tensile Strength at Break, TD | 76.0 MPa | 11000 psi | ASTM D882 |
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.The SF (Super Formable) films are modified blends of nylon 6,6 which enhance the thermoforming characteristic of the Dartek® F series of films Can be used.. |
|||
Film Tensile Strength at Break, TD | >= 76.1 MPa | >= 11000 psi | 350 N/10mm |
Dr. D. Mueller Flexiso® DMD FI 14010 00460 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00460 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Film Tensile Strength at Break, TD | 75.8 MPa | 11000 psi | ASTM D882 |
Honeywell Stretch-Vac® Elastomax 1000 Heat-Stabilized Blown Film
(discontinued **) Description: Capran® Elastomax 1000 is a pink tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 80 inches as layflat tubing and 120 inches as s.. |
|||
Film Tensile Strength at Break, TD | 75.8 MPa | 11000 psi | ASTM D882 |
ExxonMobil Exceed™ 3527PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3527PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 3527PA have high modulus and outstanding tensile, impact and puncture resistance properties. These.. |