Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 670 g | 1.48 lb | ASTM D1709 |
ExxonMobil Exceed™ 2018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018HA is a metallocene Catalyzed ethylene-hexene copolymer. Films made from Exceed 2018HA have outstanding tensile, impact strength, and puncture. These superior strengt.. |