Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 600 g | 1.32 lb | Impact Strength, ASTM D1709-62T |
DuPont™ Dartek® B-601 Nylon 6,6 Barrier Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A strong transparent nylon type 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. Can be pri.. |
|||
Dart Drop Test | 600 g | 1.32 lb | Impact Strength, ASTM D1709-62T |
DuPont™ Dartek® F-101 Nylon 6,6 Forming Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A cast nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylen diamine. It contains all the excellent properties .. |
|||
Dart Drop Test | 600 g | 1.32 lb | Impact Strength, ASTM D1709-62T |
DuPont™ Dartek® B-602 Nylon 6,6 Barrier Film, 38 µm Thickness, PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, transparent nylon 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. It is special.. |
|||
Dart Drop Test | 600 g | 1.32 lb | ISO 7765-1 |
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt.. |
|||
Dart Drop Test | 600 g | 1.32 lb | ASTM D1709 |
ExxonMobil Exceed™ 2018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018KB is a metallocene catalyzed ethylene-hexene copolymer. Films made from Exceed 2018KB have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Dart Drop Test | 600 g | 1.32 lb | ASTM-D1709 (Method B) |
Braskem TN2006 EVA General Film Copolymer TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. .. |