Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 590 g | 1.30 lb | ASTM D1709 |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Dart Drop Test | 590 g | 1.30 lb | ASTM D1709 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Dart Drop Test | 590 g | 1.30 lb | ASTM D1709 |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Dart Drop Test | 590 g | 1.30 lb | ASTM D1709 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |