Mechanical Properties Metric English Comments
Dart Drop Test 395 g
0.871 lb
(method A); ASTM D1709
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film
The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu..
Dart Drop Test 395 g
0.871 lb
(method A); ASTM D1709
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film
Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil..