Polymer Property : Dart Drop Test = 2.65 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 1200 g
2.65 lb
ASTM D1709A
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin
Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe..
Dart Drop Test 1200 g
2.65 lb
ASTM D1709A
ExxonMobil Exact™ 4160 Series Ethylene-based Plastomer Resin
Product Description: Exact 4160 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. These resins are designed for blown film applications requir..