Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 1200 g | 2.65 lb | ASTM D1709A |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Dart Drop Test | 1200 g | 2.65 lb | ASTM D1709A |
ExxonMobil Exact™ 4160 Series Ethylene-based Plastomer Resin Product Description: Exact 4160 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. These resins are designed for blown film applications requir.. |